OVERVIEW SPECIFICATIONS AND TECHNICAL INFORMATION
See Stainless Steel Tolerances
Stainless Sheet/Plate 321 provides high strength, high temperature capability, and resistance to intergranular corrosion. 321 resists scaling at higher temperatures. Also, the addition of titanium means that welding is not suggested for this alloy. It is typically used in aerospace and defense for engine parts, heat exchangers, missile components, exhaust stacks, rocket engines, manifolds, and more.

Dimension Name |
Specification |
Alloy | 321 |
Gauge | 7 ga. |
Thickness | 0.1875 |
Max Width | 48 |
Max Length | 120 |
Eniteo Vendor ID | 1582 |
MTR Availability | Yes |
Full Length | true |
Material | Stainless Steel |
Shape | Sheet/Plate |
Custom Cut Warehouse | 1 |
This material meets the following specs: ASTM -A240, ASTM -A480, AMS -5510
Weight/Lineal Foot |
||
7.75 pounds |
Mechanical Properties |
|
Property | Value |
Brinell Hardness | 200 min |
Electrical resistivity 68 F | 72 min |
Density g/cm^3 | 8 |
Elongation | 55 min |
Impact values - Izod | 80 min |
Magnetic permeability | 1 min |
Max operating temperature Intermittent | 1600 |
Max operating temperature Continuous | 1700 |
Mean Coefficient of Expansion 68-212F | 8 min |
Mean Coefficient of Expansion 68 to indicated-ºF | 10 min |
Melting Point | 2550 min |
Modulus of elasticity | 29 min |
Reduction of Area % | 65 min |
Rockwell Hardness | 95 min |
Thermal conductivity 212 F | 9 min |
Specific Heat BTU/lb-°F (32-212F) | 1 |
Thermal conductivity 932 F | 12 min |
Ultimate Tensile Strength | 85 min |
Yield | 35 min |
Chemistry Information: 321 Stainless Steel |
|
Element | Percentage |
C | 0.08 |
Cr | 18 |
Fe | 68 |
Mn | 2 |
P | 0.045 |
S | 0.03 |
Ni | 11 |
Si | 1 |
Ti | 0.15 |