Product Details, Specifications, and Technical Information
See Stainless Steel Tolerances
Stainless Sheet/Plate 347 provides high strength, high temperature capability, and corrosion resistance in strongly oxidizing environments. 347 is an austenitic stainless and also can operate at high temperatures without losing strength. It is typically used in aerospace for aircraft exhausts, collector rings, expansion joints, and in high temperature chemical processing.
Dimension Name | Specification |
Thickness | 0.25 |
Max Width | 48 |
Max Length | 120 |
Alloy | 347 |
Covering | Pvc 1 Side |
Eniteo Vendor ID | 3143 |
MTR Availability | Yes |
Full Length | true |
Material | Stainless Steel |
Shape | Sheet/Plate |
Custom Cut Warehouse | 1 |
Material Specifications
This material meets the following specs: ASTM -A262, ASTM -A240, AMS -5512
Weight/Lineal Foot | ||
10.34 pounds |
Please note that this data is to be used ONLY FOR REFERENCE, NOT FOR DESIGN, and by using it,you agree that any decisions you make regarding materials for your project are at your own discretion.
Mechanical Properties | |
Property | Value |
Yield Tensile Strength KSI | 39 |
Ultimate Tensile Strength KSI | 93 |
Rockwell Hardness B Scale | 85 |
Density g/cm^3 | 8 |
Shear Strength KSI | 65 |
Brinell Hardness 500 kg load | 167 |
Melting Point °F | 2550 - 2600 |
Machinability % | 36 |
Elongation % in 2 in. | 45 |
Electrical Conductivity % IACS | 2 |
Chemistry Information: 347 Stainless Steel | |
Element | Percentage |
Mn | 2 max |
C | 0.08 max |
P | 0.045 max |
S | 0.03 max |
Si | 0.75 max |
Cr | 17 - 19 |
Ni | 9 - 13 |
Nb + Ta | 1 max |